Material | Hardness (HRC) | Impact Toughness (J/cm2) | Application | Standards |
M05 | ≥58 | 5~7 | Alloy M05 is particularly suited for greater impact load and fair corrosion resistance, and it is used when pH range is 5-12. | ASTM A532 CL III - A |
M07 | ≥58 | 5~7 | Alloy M07 has lower wear resistance but higher impact resistance than alloy M05. It is used when pH range is 5-12. | ASTM A532 CL III - A |
M10 | ≥58 | 5~7 | Known as 1821 white iron, widely used in mining industry as most efficient and cost effective option. | AS 2027 -2007 |
Material | Hardness (HRC) | Impact Toughness (J/cm2) | Application | Standards |
M05 | ≥58 | 5~7 | Alloy M05 is particularly suited for greater impact load and fair corrosion resistance, and it is used when pH range is 5-12. | ASTM A532 CL III - A |
M07 | ≥58 | 5~7 | Alloy M07 has lower wear resistance but higher impact resistance than alloy M05. It is used when pH range is 5-12. | ASTM A532 CL III - A |
M10 | ≥58 | 5~7 | Known as 1821 white iron, widely used in mining industry as most efficient and cost effective option. | AS 2027 -2007 |